Injection & Extrusion Cylinder

01Outline of Cylinder (Barrel)

The cylinder as a heating unit must be thermally stable (cylinder wall thickness) to maintain constant melt temperature. In addition, very high level of straightness (+0.02) is required to prevent generation of over heat while the screw is rotating.

02Cylinder Wear

Cylinder wear is caused by the friction at the screw head (last Front 4D), corrosive gas, and the friction at the resin feed throat (first 5D) for metering.

Max. allowable wear

Low viscosity resin -0.1mm, High viscosity resin -0.2mm

03Cylinder Selection

More and more highly abrasive compounds reinforced with glass fiber or filler and super engineering plastics are developed and used. To this end, the cylinders must be made with the materials highly resistant to wear and corrosion.

04Classification by Material

Material Use Remark
Cylinder SACM645 General Universal resins
ALLOY(Fe-Base) High resistance to wear Wear resistant (GF 10%)
ALLOY(Ni-Base) Resistant to wear & corrosion Wear & corrosion resistant (GF 30%)
ALLOY(W-Base) Super-high resistance to wear & corrosion Special specification (GF 10%)